堆肥条件下生物降解性的评价体系--EN13432 详解
EN 13432 Packaging - Requirements for packaging recoverable through composting and biodegradation - Test scheme and evaluation criteria for the final acceptance of packaging
Scope:packaging and packaging materials(包装及包装材料)
Remark: 包装含多种组成部分,其中有不可堆肥的部分,则整体认为不可堆肥,除非可手动分离。
后台回复13432,获得中文版
1.Control of Constituents:评价材料本身的特性
(1)Packaging,packaging materials and packaging components shall contain a minimum of 50% of volatile solids which exclude largely inert materials.(大于50%的挥发性物质)
(2)Heavy metals and other toxic and hazardous substances(评估重金属或其他有毒有害物质)
(3)Determination of the organic carbon content, total dry solids and volatile solids of the packaging material used for biodegradation and disintegration tests.(总有机碳含量,干物质总量,挥发性物质总量)
2.Biodegradability:生物降解能力
(1)Significant organic constituents:any organic constituent present in more than 1% of dry weight of that material. The total proportion of organic constituents without determined biodegradability shall not exceed 5%. (超过1%的成分都需要测试生物降解能力,小于1%的部分总和不超过5%)
(2)Chemically unmodified packaging materials and constituents of natural origin, such as wood, wood fibre, cotton fibre, starch, paper pulp or jute shall be accepted as being biodegradable without testing. (未经过化学改性或纯天然的材料,如纸浆、淀粉、棉麻纤维、木及木头纤维或黄麻可以不经测试被认为生物可降解)
(3)Aerobic biodegradation tests 需氧生物降解测试测试
周期不得超过6个月,生物降解率超过90%
(4)Anaerobic biodegradation tests 厌氧生物降解测试测试
周期不得超过2个月,生物降解率超过50%
3.Disintegration:崩解能力
(1)Unless technically impossible the packaging, packaging material or packaging component shall be tested for disintegration in the form in which it will ultimately be used. 崩解应该以最终的使用状态进行测试
In practice packaging materials are tested and from this it is concluded that a complete packaging will be disintegrated if all of its materials are capable of disintegration. A complete packaging should, however, be tested in cases where a direct conclusion is not possible e.g. if two or more packaging materials are firmly joined together forming a fixed multi-layer structure.
如果两种或多种材料通过复合在一起形成了稳定的过程结构,完整包装需要整体测试崩解能力
(2)未经过化学改性或纯天然的材料也需要测试崩解能力。
(3)Aerobic biodegradation tests 需氧生物降解测试测试
周期不得超过12个周,90%要通过2mm筛子
(4)Anaerobic biodegradation tests 厌氧生物降解测试测试
周期不得超过5个周,90%要通过2mm筛子
4.Compost quality:堆肥质量
(1)Physical-chemical parameters 理化性质
(volumetric weight (density), total dry solids, volatile solids, salt content,PH, total nitrogen, ammonium nitrogen, phosphorus, magnesium and potassium)
(2)Ecotoxicity 生态毒性
The germination rate and the plant biomass of the sample composts of both plant species should be more than 90 % of those from the corresponding blank compost (see Annex E).
两种植物的发芽率和植物重应超过空白堆肥的90%
测试方法
OECD 208: Terrestrial Plant Test - Seedling Emergence and Seedling Growth Test
数据有效性
(1) 出苗率应不少于70%;
(2)幼苗没有可见的植物毒素影响(如变色病、坏死病、枯萎、叶子和茎的畸形),个别种类的植株在生长和形态上只有正常变异;
(3) 试验期间,对照组幼苗平均存活率应高于90%;
(4)特定品种的生长环境条件应保持一致,同时其生长介质中应含有等量的人工土壤基质、支持介质或同样来源的基质。
添加好友请备注:姓名+公司+主营
5.Exemptions:可豁免的
(1)Equivalent form(等价形式)
A packaging material demonstrated to be organically recoverable in a particular form, shall be accepted as being organically recoverable in any other form having the same or a smaller mass to surface ratio or wall thickness. 已经证明在某一特定形式下是有机可回收的,其更小的面积和厚度可以等价为有机可回收。
(2) Materials of natural origin(天然来源的材料)
Chemically unmodified packaging materials and constituents of natural origin, such as wood, wood fibre, cotton fibre, starch, paper pulp or jute shall be accepted as being biodegradable without testing (see clause 6) but shall be chemically characterized (see 4.2) and fulfil the criteria for disintegration (see clause 7) andcompost quality . 未经过化学改性或纯天然的材料,如纸浆、淀粉、棉麻纤维、木及木头纤维或黄麻可以不经测试被认为是生物可降解,但需要测试理化性质,崩解能力和堆肥质量。
来源:迟延娜《生物降解材料及制品的可堆肥能力检测认证及合规要求》
→ 海南白名单 | 宁波家联科技 | 深圳裕同科技 | 广东天元股份 | 海南样板 | 美团白名单 | 上海永冠新材 | 安徽瑞鸿新材料→ 吹膜工艺大全 | 餐盒工艺 | 吸管工艺 | PLA吹膜工艺 | PBSA/PLA+淀粉 | PE+淀粉工艺 | PP+淀粉工艺【标准】→ 新版国标20197删除光氧 全文 jj标识 规范指南 光氧被除名 PE+淀粉不是全降解 每一种都应全降解 旧版20197全文 | 云南光氧降解 也用jj | 四川引导全降解 | 上海引导全降解 | 江苏引导全降解 | 浙江宁波引导全降解 | 安徽宿州光氧-生物酶 | 海南禁塑名录 | 海南核磁法/图谱法 | 浙江绿色包装地标 | 农膜管理办法 | 推荐国标法律效力 | 生物降解塑料购物袋38082 | 淀粉基38079 PE+淀粉工艺 | 塑料购物袋21661 | 用哪个标准| 一次性可降解餐饮具18006.3 | 欧盟EN13432 解读 | 英国定义可生物降解PSA9017 |
→ 检测方法 | 国内标准 | 国际标准 | 标准和认证 | 美国BPI认证 | 欧盟DIN | 日本 | 澳大利亚 | 快速检测法【观点】→ 意见分歧 | 人民日报:不搞一刀切 解读 | 工信部鼓励全降解 | 亟待标准 | 翁云宣 4R1D | 夏青 | 王玉忠 |季君晖 | 王文广 | 卢波 | 甄光明 | 北石化院报告 | 德国大学 | 绿色和平呼吁降温 | 降解圈乱象 | 光氧降解出路 | 降解剂在美被罚 | 降解剂浑水摸鱼? | 食入微塑料 | 伪降解 | 瑞力恒被举报 | 假环保袋 | 纸杯防油剂含氟 | 谁是主流 | 谁主导市场 | 部分降解退场 | 替代还是改良 | PBAT不能生物降解? | PTA有没有害 | PLA糟蹋粮食? | PLA&粮食 | PLA海水不降解 | PBS替代PLA | 石油基&生物基 | 厌氧降解 | 堆肥厂100个 | 国标落后15年 | 旧版失败原因 | 新版难成功? | 降解不能包治百病 | 不是万灵药 | 降解PK纸包装 | 海南全焚烧 | 降解塑料应焚烧 | 降解塑料也要分类【政策】→ 各省政策表 | 方案秘密 | 禁用EPS | 商务部报告系统 | 海南监管码 | 海南5项经验 | 5省市0填埋 | 国家邮政局 | 电商需停用不可降解袋 | 快递绿色包装标志 | 餐饮禁塑PK | 国外禁塑政策 | 美国 | 欧盟禁止OXO | 欧盟塑料税 | 西班牙 | 英国 | 加拿大 | 肯尼亚 | 新西兰【研报】→ 研报第3版印刷版 | 31只概念股 | 8家龙头 | 产业链全景 | 十年千亿 | 降解名人堂 | 院校专业 | 发展简史| 科普解读 | 图解 | 术语 | 降解塑料15问 | 应用领域 | 包装前景【工艺】→ PBAT合成 | PLA+PBAT+扩链剂 | PBAT共混改性 | 硅灰石填充 | 碳酸钙填充 | PBAT地膜 | PBAT吹膜有黑点→ PLA结晶 | PLA淋膜 | PLA成核改性 | PLA发泡片材 | 发泡工艺 | PLA发泡50倍 | CO2超临界发泡 | PLA发泡机械重要性 | PLA发泡最新成果 | 金丹科技合成丙交酯 | 扩链法合成PLA | PLA开环聚合 | L-PLA聚合| 成核剂提高结晶 | PLA增韧 | 酚氧树脂填充 | PLA复合膜 | PLA装沸水 | 丙交酯卡脖子 | PLA物理和化学改性 | PLA纤维 | PLA平膜法→ PBS合成 | PBS发泡 | 季君晖海水降解 | 季君晖合金改性→ PHA合成 | 陈国强PHA | 蓝晶PHA→ 淀粉基前景 | 淀粉物理改性 | 淀粉化学改性 | 交联淀粉 | 淀粉基塑料→ PCL合成 | 王玉忠PPDO | PPC | PPC力争第三 | 浦景化工PGA | PBTL | 【前沿】→ 王玉忠升级回收 | 俞书宏仿生材料 仿生膜 | PLA最新专利 | NW丙交酯提升10% | 道达尔PLA回收 | 塞拉尼斯纤维素 | LG生物材料 | 苏伊士回收PE | 中国PLA+石墨烯 | 中国PLA+TPU | 韩国PLA+PVC共混 | 新西兰PLA+PE共混 | 新加坡PLA+橡胶 | 伊朗PVC绿色增塑剂 | 纤维餐具 | 废塑料热解油化 | 纸杯微塑料 | 水性涂层 | PET水解酶 | PET超级酶 | PU降解菌 | 黑水虻 | 蜡虫 | 硫脲 | 嗜盐微生物 | 酶蛋白 | 甲壳素 | 壳聚糖